Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 4.31 MPa | >= 625 psi | Stabilized, min |
Hexcel® HexWeb® HRH-327 - 3/16 - 6.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |