Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 2.00 - 4.00 MPa @Strain 1.00 % |
290 - 580 psi @Strain 1.00 % |
ASTM D695 |
Guarniflon PTFE G200 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |