Mechanical Properties Metric English Comments
Compressive Yield Strength 255 MPa
37000 psi
ASTM D695
Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 255 MPa
37000 psi
ASTM D695
Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled
Data provided by Adell Plastics, Inc.