Polymer Property : Compressive Yield Strength = 369 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 369 MPa
53500 psi
Compression After Impact @ 6.6 J/mm, Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; pr EN 6038
Hexcel® HexPly® 920CX-EP2015-47.5% 125°C Curing Epoxy Matrix
Intermediate modulus, 6K carbon, 2x2 twill, 193 g/m2Information provided by HexCel