Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 226 MPa | 32800 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |