Mechanical Properties Metric English Comments
Compressive Yield Strength 2.24 MPa
325 psi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 2.24 MPa
325 psi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength >= 2.24 MPa
>= 325 psi
Stabilized, min
Hexcel® HexWeb® HRH-327 - 3/8 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Compressive Yield Strength >= 2.24 MPa
>= 325 psi
Stabilized, min
Hexcel® HexWeb® HRP - 3/8 - 3.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..