Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 31.7 MPa @Strain 1.00 %, Time 3.60e+6 sec |
4600 psi @Strain 1.00 %, Time 1000 hour |
ASTM D695 |
Manifattura Cattaneo VESPEL® SP22 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |