Polymer Property : Compressive Yield Strength = 30500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 210 MPa
30500 psi
Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated
SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p..