Compressive Yield Strength >= 3.65 MPa
>= 530 psi
Bare, min
Hexcel® HexWeb® HRP - 1/4 - 5.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Yield Strength >= 3.65 MPa
>= 530 psi
Stabilized, min
Hexcel® HexWeb® HRP - 3/8 - 4.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..