Polymer Property : Compressive Yield Strength = 3.24 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 3.24 MPa
>= 470 psi
Stabilized, min
Hexcel® HexWeb® HRH-10 - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength >= 3.24 MPa
>= 470 psi
Stabilized, min
Hexcel® HexWeb® HRP/F35 - 4.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Compressive Yield Strength >= 3.24 MPa
>= 470 psi
Stabilized, min
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength >= 3.24 MPa
>= 470 psi
Stabilized, min
Hexcel® HexWeb® HRH-10/F50 - 4.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Compressive Yield Strength >= 3.24 MPa
>= 470 psi
Stabilized, min
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..