Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0207 MPa

@Strain 25.0 %
3.00 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Handheld Urethane Foam, Handheld Grade, PET Reinforced
Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent..
Compressive Yield Strength 0.0207 MPa
3.00 psi
At 10% compression
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Compressive Yield Strength 0.0207 MPa
3.00 psi
At 10% compression
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Compressive Yield Strength 0.0207 MPa
3.00 psi
At 10% compression
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Compressive Yield Strength 0.0207 MPa
3.00 psi
At 10% compression
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..