Polymer Property : Compressive Yield Strength = 28880 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 199.1 MPa
28880 psi
ASTM D695
Plenco 4246 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use..