Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 124 - 198 MPa | 18000 - 28700 psi | Average value: 175 MPa Grade Count:7 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |