Mechanical Properties Metric English Comments
Compressive Yield Strength 197.8 MPa
28690 psi
ASTM D695
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol..