Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 26.0 - 138 MPa | 3770 - 20000 psi | Average value: 87.0 MPa Grade Count:11 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Compressive Yield Strength | 26.0 MPa @Strain 1.00 % |
3770 psi @Strain 1.00 % |
ISO 604 |
Manifattura Cattaneo PA 6 G Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Compressive Yield Strength | 26.0 MPa @Strain 1.00 % |
3770 psi @Strain 1.00 % |
ISO 604 |
Manifattura Cattaneo PET Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |