Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 45.0 - 250 MPa @Temperature 120 - 250 °C |
6530 - 36300 psi @Temperature 248 - 482 °F |
Average value: 125 MPa Grade Count:10 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Compressive Yield Strength | 4.14 - 250 MPa | 600 - 36300 psi | Average value: 181 MPa Grade Count:21 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Compressive Yield Strength | 142 - 250 MPa | 20600 - 36300 psi | Average value: 194 MPa Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |