Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 243 MPa | 35200 psi | Compression After Impact, 20J |
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix, Unidirectional Prepreg Laminate (M36/32%/135/HTA) Tenax HTA fiberInformation provided by HexCel |