Polymer Property : Compressive Yield Strength = 24.7 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.170 MPa
24.7 psi
at 20% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ F DF-225A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 70Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Compressive Yield Strength 0.170 MPa
24.7 psi
at 10% Compression, Parallel to thickness
Zircar Ceramics ECO-1200A Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provid..
Compressive Yield Strength 0.170 MPa
24.7 psi
Compressive Load Deflection at 5%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2590 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..