Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 2.00 - 24.1 MPa | 290 - 3500 psi | Average value: 7.31 MPa Grade Count:10 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |