Polymer Property : Compressive Yield Strength = 23310 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 160.7 MPa
23310 psi
ASTM D695
Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..