Mechanical Properties Metric English Comments
Compressive Yield Strength 226.1 MPa
32790 psi
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy
This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%..