Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 219000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 1510 MPa
219000 psi
Hexcel® HexPly® EH04 Epoxy Resin System, Fortafil 510 Fiber
F510 150 24" EH04 38%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Compressive Yield Strength 1510 MPa
219000 psi
Hexcel® HexPly® EH04 Epoxy Resin System, M35J Fiber
MS35J 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Compressive Yield Strength 1510 MPa

@Temperature 23.0 °C
219000 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, G40-800 Fiber
Information provided by HexCel
Copyright © lookpolymers.com All Rights Reserved