Mechanical Properties Metric English Comments
Compressive Yield Strength 1.50 - 23.4 MPa
218 - 3400 psi
Average value: 7.20 MPa Grade Count:23
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Compressive Yield Strength 1.50 MPa
218 psi
Stabilised
Hexcel® HexWeb® CRF-1/2-ACG-.003-2.6 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..
Compressive Yield Strength 1.50 MPa
218 psi
ASTM C365
Parabeam Industrie Paraglass 10 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..