Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 214 MPa | 31000 psi | ASTM D695 |
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Yield Strength | 214 MPa | 31000 psi | 90º, RT, Dry; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |