Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 147 MPa | 21300 psi | |
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif.. |