Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 139 - 213 MPa | 20200 - 30900 psi | Average value: 175 MPa Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |