Mechanical Properties Metric English Comments
Compressive Yield Strength 144 - 169 MPa
20800 - 24500 psi
Average value: 160 MPa Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..