Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 4100 Phenolic, Granular, Compression Molded
(discontinued **) Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and .. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 204 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to accommodate a wide range of molding situations. In addition, it is recommended for use in thin wall .. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range .. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok 304 is a two-stage, woodflour and cellulose-filled phenolic molding compound having improved impact strength. It is suitable for automatic molding, and is recommended for thin-walled parts .. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 306 Black General Purpose Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 306 is a two-stage, mineral and flock-filled phenolic molding compound designed to have the heat resistant characteristics of Plaslok 504, while at the same time, improved impact strength.Da.. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Adell AR-34 Nylon 66, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Adell BR-38 Nylon 6, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T33J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2,3.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T357 Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T359J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 3, 14.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Adell AR-14 Nylon 66, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Adell BR-18 Nylon 6, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties... |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plaslok 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5440 is the replacement material for .. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo.. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plaslok 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 304 is a two-stage, woodflour and cel.. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plaslok 306 Black General Purpose Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 306 is a two-stage, mineral and flock.. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T385J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 207 MPa | 30000 psi | ASTM D695 |
Plaslok 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 204 is a two-stage, woodflour and min.. |