Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 206.2 MPa | 29910 psi | ASTM D695 |
Plenco 7300 Phenolic, Nodular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |