Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 2.50 MPa | 363 psi | Stabilised |
Hexcel® HexWeb® CRF-1/4-ACG-.002-3.4 Chromate free ACG® Honeycomb Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app.. |