Mechanical Properties Metric English Comments
Compressive Yield Strength 2.30 MPa
334 psi
Sawbones Cellular Rigid Polyurethane Foam 10 pcf Density
Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone ..