Polymer Property : Compressive Yield Strength = 199.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 199.7 MPa
28960 psi
ASTM D695
Plenco 2424 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical ..