Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 193.7 MPa | 28090 psi | ASTM D695 |
Plenco 50045 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |