Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1900 MPa | 276000 psi | 0.2%, hardened to 55 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Compressive Yield Strength | 1900 MPa | 276000 psi | Rc0.2. Hardness HRC 56. |
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |