Mechanical Properties Metric English Comments
Compressive Yield Strength 186 MPa
27000 psi
ASTM D695
Adell BH-18 Nylon 6, 40% Mineral Filled
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 186 MPa
27000 psi
ASTM D695
Adell BH-38 Nylon 6, 40% Mineral Filled
Data provided by Adell Plastics, Inc.