Polymer Property : Compressive Yield Strength = 18500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 128 MPa
18500 psi
Perpendicular to Laminate
TriStar Ultracomp UC-200 Composite Bearing
Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m..
Compressive Yield Strength 128 MPa
18500 psi
Perpendicular to Laminate
TriStar Ultracomp UC-500 Composite Bearing
Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear li..