Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1800 MPa | 261000 psi | 0.2%, hardened to 55 HRC |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
Compressive Yield Strength | 1800 MPa | 261000 psi | 0.2%, Aged to ~ 50 HRC |
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli.. |
|||
Compressive Yield Strength | 1800 MPa | 261000 psi | 0.2%, hardened to 55 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |