Compressive Yield Strength 350 - 1786 MPa

@Temperature -59.0 - 150 °C
50800 - 259000 psi

@Temperature -74.2 - 302 °F
Average value: 888 MPa Grade Count:26
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..