Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 175.7 MPa | 25480 psi | ASTM D695 |
Plenco 51030 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued.. |