Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 11.62 MPa | >= 1685 psi | Stabilized, min, preliminary |
Hexcel® HexWeb® CR III 1/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |