Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 68.9 - 165 MPa | 10000 - 23900 psi | Average value: 114 MPa Grade Count:20 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |