Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1640 MPa | 238000 psi | 0.2%; Average Longitudinal Hardened |
ATI Allegheny Ludlum K12® Dual Hardness Steel This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp.. |