Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.110 MPa | 16.0 psi | at 10% Compression, Parallel to thickness |
Zircar Ceramics ECO-20AA Alumina Insulation ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.110 MPa @Strain 10.0 % |
16.0 psi @Strain 10.0 % |
Parallel to Thickness |
Zircar Ceramics Uniform A1 Alumina-Silica Insulation ZIRCAR Alumina-Silica Insulation Type "UNIFORM A" is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi.. |
|||
Compressive Yield Strength | 0.110 MPa @Strain 50.0 % |
16.0 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 304 CM-HD EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.110 MPa @Strain 25.0 % |
16.0 psi @Strain 25.0 % |
ASTM D1056 |
Rogers Corporation Bisco® L3 Premiere Next Generation Dynamic Flooring Material BISCO® L3 Premiere silicone foam technology is the next generation in dynamic and floating floor materials from Rogers Corporation developed specifically to meet the most challenging global require.. |