Mechanical Properties Metric English Comments
Compressive Yield Strength 15.0 MPa
2180 psi
at 2% nominal strain; ISO 604
Quadrant EPP Cesticolor™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Compressive Yield Strength 15.0 MPa
2180 psi
at 2% nominal strain; ISO 604
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Compressive Yield Strength 15.0 MPa
2180 psi
at 5% nominal strain; ISO 604
Quadrant EPP Cestlite™ ASTL Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.