Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 9.70 MPa | 1410 psi | at 10% deflection, parallel to thickness |
Zircar Refractory Composites RS-A2 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |