Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 965 MPa @Temperature 23.0 °C |
140000 psi @Temperature 73.4 °F |
0º, 120°C Cure, Conditioning: 23°C; ASTM D965 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre 1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel |
|||
Compressive Yield Strength | 965 MPa | 140000 psi | |
Materion moldMAX® LH High Hardness Beryllium Copper Alloy Description: moldMAX® and PROtherm® are Brush Wellman's copper beryllium alloys specifically designed for the plastic processing industry. These alloys provide a combination of thermal conduct.. |