Polymer Property : Compressive Yield Strength = 130 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 130 - 200 MPa
18900 - 29000 psi
Average value: 165 MPa Grade Count:34
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Compressive Yield Strength 130 MPa
18900 psi
ASTM D695
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf..
Compressive Yield Strength 130 MPa
18900 psi
RT; Dry; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel