Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 850 MPa @Temperature 75.0 °C |
123000 psi @Temperature 167 °F |
Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |