Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 12.9 MPa @Strain 10.0 % |
1870 psi @Strain 10.0 % |
|
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Compressive Yield Strength | 12.9 MPa @Strain 10.0 % |
1870 psi @Strain 10.0 % |
|
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |