Mechanical Properties Metric English Comments
Compressive Yield Strength 8.00 MPa
1160 psi
at 2% nominal strain; ISO 604
Quadrant EPP Cestilene™ HD 1000 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Compressive Yield Strength 8.00 - 9.00 MPa

@Strain 1.00 %
1160 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..
Compressive Yield Strength 8.00 MPa
1160 psi
Typical; ASTM C365
Parabeam Industrie ParaTank 3 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..